Schädigungsmodell für die Hydroabrasionsbeanspruchung zur probabilistischen Lebensdauerprognose von Betonoberflächen im Wasserbau
Hydraulic structures are exposed to multifaceted exposures. Particular the hydro-abrasive wear of the concrete edge zones represents a key exposure. The knowledge about the abrasive mechanisms of concrete and its degradation process is still insufficient. Relating to the hydro-abrasive test method,...
Saved in:
Main Author: | |
---|---|
Format: | Electronic Book Chapter |
Published: |
KIT Scientific Publishing
2017
|
Series: | Karlsruher Reihe Massivbau, Baustofftechnologie, Materialprüfung / Institut für Massivbau und Baustofftechnologie ; Materialprüfungs- und Forschungsanstalt Karlsruhe
|
Subjects: | |
Online Access: | DOAB: download the publication DOAB: description of the publication |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
MARC
LEADER | 00000naaaa2200000uu 4500 | ||
---|---|---|---|
001 | doab_20_500_12854_58936 | ||
005 | 20210212 | ||
003 | oapen | ||
006 | m o d | ||
007 | cr|mn|---annan | ||
008 | 20210212s2017 xx |||||o ||| 0|deu d | ||
020 | |a KSP/1000054428 | ||
020 | |a 9783731505228 | ||
040 | |a oapen |c oapen | ||
024 | 7 | |a 10.5445/KSP/1000054428 |c doi | |
041 | 0 | |a deu | |
042 | |a dc | ||
072 | 7 | |a TBX |2 bicssc | |
100 | 1 | |a Vogel, Michael |4 auth | |
245 | 1 | 0 | |a Schädigungsmodell für die Hydroabrasionsbeanspruchung zur probabilistischen Lebensdauerprognose von Betonoberflächen im Wasserbau |
260 | |b KIT Scientific Publishing |c 2017 | ||
300 | |a 1 electronic resource (Getr. Zählung p.) | ||
336 | |a text |b txt |2 rdacontent | ||
337 | |a computer |b c |2 rdamedia | ||
338 | |a online resource |b cr |2 rdacarrier | ||
490 | 1 | |a Karlsruher Reihe Massivbau, Baustofftechnologie, Materialprüfung / Institut für Massivbau und Baustofftechnologie ; Materialprüfungs- und Forschungsanstalt Karlsruhe | |
506 | 0 | |a Open Access |2 star |f Unrestricted online access | |
520 | |a Hydraulic structures are exposed to multifaceted exposures. Particular the hydro-abrasive wear of the concrete edge zones represents a key exposure. The knowledge about the abrasive mechanisms of concrete and its degradation process is still insufficient. Relating to the hydro-abrasive test method, the relevant material parameter and degradation model incomplete knowledge existed which was removed. | ||
540 | |a Creative Commons |f https://creativecommons.org/licenses/by-sa/4.0/ |2 cc |4 https://creativecommons.org/licenses/by-sa/4.0/ | ||
546 | |a German | ||
650 | 7 | |a History of engineering & technology |2 bicssc | |
653 | |a Beton | ||
653 | |a Lebensdauer | ||
653 | |a Test method | ||
653 | |a Hydroabrasionsverschleiß | ||
653 | |a Concrete | ||
653 | |a SchädigungsmodellHydro-abrasion | ||
653 | |a Prüftechnik | ||
653 | |a Life-time | ||
653 | |a Deterioration model | ||
856 | 4 | 0 | |a www.oapen.org |u https://www.ksp.kit.edu/9783731505228 |7 0 |z DOAB: download the publication |
856 | 4 | 0 | |a www.oapen.org |u https://directory.doabooks.org/handle/20.500.12854/58936 |7 0 |z DOAB: description of the publication |