The Effects of Coffee and Energy Drink on Color Stability of Hybrid Ceramics

Purpose: The aim of this study was to compare the color stability of two different hybrid ceramic materials.Materials amp; Methods: Using the precision cutting device (Micracut, Metcon, Turkey), 36 specimens (12 x 15 x 1 mm) were obtained from Vita Enamic (Vita Zahnfabrik, Germany) and Lava Ultimate...

Full description

Saved in:
Bibliographic Details
Main Authors: Hande Yıldız Dilli (Author), Işıl Sarıkaya (Author)
Format: Book
Published: Ankara University, 2021-04-01T00:00:00Z.
Subjects:
Online Access:Connect to this object online.
Tags: Add Tag
No Tags, Be the first to tag this record!

MARC

LEADER 00000 am a22000003u 4500
001 doaj_3f1f9fcb667f43399a3e66b0cfd6f23b
042 |a dc 
100 1 0 |a Hande Yıldız Dilli  |e author 
700 1 0 |a Işıl Sarıkaya  |e author 
245 0 0 |a The Effects of Coffee and Energy Drink on Color Stability of Hybrid Ceramics 
260 |b Ankara University,   |c 2021-04-01T00:00:00Z. 
500 |a 2757-6744 
500 |a 10.52037/eads.2021.0006 
520 |a Purpose: The aim of this study was to compare the color stability of two different hybrid ceramic materials.Materials amp; Methods: Using the precision cutting device (Micracut, Metcon, Turkey), 36 specimens (12 x 15 x 1 mm) were obtained from Vita Enamic (Vita Zahnfabrik, Germany) and Lava Ultimate (3M ESPE, St.Paul, USA) CAD / CAM blocks. After finishing procedures were completed, all specimens were stored in distilled water for 24 h. Then, the specimens were dried and the initial color measurements were made. L, a, b values were determined using a spectrophotometer (Vita Easy Shade, Vita Zahnfabrik, Germany). The specimens were then divided into 3 test groups and stored in coffee (Nescafe Classic, Turkey) (G2, G5), energy drink (Red Bull, Austria) (G3, G6), and in the distilled water as the control group (G1, G4), for 48 h. After 48 h, the specimens were washed with distilled water and dried. Second color measurements were made. ∆E00 values were calculated using the CIEDE 2000 color-difference formula.Results: Data were analyzed by two-way ANOVA. Multiple comparisons were made with Bonferroni's test. There was a statistically significant difference between 2 ceramics (p=0.035). Generally, Lava Ultimate showed more color change than Vita Enamic. Among the beverages, coffee was significantly different for both ceramics than control and energy drink (p lt;0.05).Conclusion: Lava Ultimate, showed more color change than Vita Enamic. Coffee has also been determined as the most colorant drink for both hybrid ceramics. 
546 |a EN 
690 |a ciede 2000 
690 |a color stability 
690 |a hybrid ceramic 
690 |a resin nanoceramic 
690 |a Dentistry 
690 |a RK1-715 
655 7 |a article  |2 local 
786 0 |n European Annals of Dental Sciences, Vol 48, Iss 1, Pp 18-22 (2021) 
787 0 |n https://dergipark.org.tr/en/download/article-file/1555516 
787 0 |n https://doaj.org/toc/2757-6744 
856 4 1 |u https://doaj.org/article/3f1f9fcb667f43399a3e66b0cfd6f23b  |z Connect to this object online.