Effect Of Surface Treatment on Shear Bond Strength of Acrylic Resin to Cobalt-Chromium Alloy

Aims: to evaluate the effect of metal primer with acid etch, laser beam, and sand blasting on shear bond strength(SBS) or resin metal and surface roughness(SR). Materials and methods: fifty Co-Cr metal plate were prepared with 10X10X1 mm dimensions. These metal plates were divided in to 5 groups con...

Full description

Saved in:
Bibliographic Details
Main Author: Mohammed M.Sadoon (Author)
Format: Book
Published: University of Mosul, College of Dentistry, 2014-08-01T00:00:00Z.
Subjects:
Online Access:Connect to this object online.
Tags: Add Tag
No Tags, Be the first to tag this record!

MARC

LEADER 00000 am a22000003u 4500
001 doaj_45121cd1dd2841f0bc44d3c9852a9ad0
042 |a dc 
100 1 0 |a Mohammed M.Sadoon  |e author 
245 0 0 |a Effect Of Surface Treatment on Shear Bond Strength of Acrylic Resin to Cobalt-Chromium Alloy 
260 |b University of Mosul, College of Dentistry,   |c 2014-08-01T00:00:00Z. 
500 |a 10.33899/rden.2014.160903 
500 |a 1812-1217 
500 |a 1998-0345 
520 |a Aims: to evaluate the effect of metal primer with acid etch, laser beam, and sand blasting on shear bond strength(SBS) or resin metal and surface roughness(SR). Materials and methods: fifty Co-Cr metal plate were prepared with 10X10X1 mm dimensions. These metal plates were divided in to 5 groups control (without treatment), acid etched with hydrochloric acid(10%) with metal primer(AP), laser beam with metal primer(LP), sand blasting with metal primer(SP), and metal primer alone(P). These groups were tested for shear bond strength of resin to metal and surface roughness. Results: there are a significant differences in shear bond strength of all treated groups in contrast to control groups, and the AP had the highest shear bond strength value. While surface roughness of tested samples shows the control group smoothest surface in relation to other groups and there is no significant difference with metal primer only and the AP group had higher surfaces roughness. Conclusion: metal primer improve bond strength between Co-Cr and chemical cured acrylic resin, the treating surface with HCL acid increase SBS and SR of metal plate. The roughening of metal surface by different treatment ( P, AP, LP, and SP) improve the SBS of metal bond to resin. 
546 |a AR 
546 |a EN 
690 |a metal primer 
690 |a shear bond strength 
690 |a surface roughness 
690 |a Dentistry 
690 |a RK1-715 
655 7 |a article  |2 local 
786 0 |n Al-Rafidain Dental Journal, Vol 14, Iss 2, Pp 252-258 (2014) 
787 0 |n https://rden.mosuljournals.com/pdf_160903_3656420070e01921465fe3596ea3e67a.html 
787 0 |n https://doaj.org/toc/1812-1217 
787 0 |n https://doaj.org/toc/1998-0345 
856 4 1 |u https://doaj.org/article/45121cd1dd2841f0bc44d3c9852a9ad0  |z Connect to this object online.