Effect of sandblasting on fracture load of titanium ceramic crowns

Purpose of the Study: It is difficult to achieve a reliable bond between the titanium and veneering porcelain. The aim of this study was to evaluate the bond strength between titanium ceramic crowns. Materials and Methods: The surfaces of titanium copings were divided in two groups. Group A sandblas...

Full description

Saved in:
Bibliographic Details
Main Authors: Arvind I Moldi (Author), Kishor Singh Bhandari (Author), Sharanbassapa Nagral (Author), Sumit Deshpandey (Author), Pawan Kulkarni (Author)
Format: Book
Published: Wolters Kluwer Medknow Publications, 2015-01-01T00:00:00Z.
Subjects:
Online Access:Connect to this object online.
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Purpose of the Study: It is difficult to achieve a reliable bond between the titanium and veneering porcelain. The aim of this study was to evaluate the bond strength between titanium ceramic crowns. Materials and Methods: The surfaces of titanium copings were divided in two groups. Group A sandblasted with 250 um (n = 10) and Group B without sandblasting (n = 10). Low-fusing porcelain was bonded over copings. A universal testing machine was used to determine the fracture load (N) of the crowns. All data were compared using Student's t-test. Results: There was a significant difference in fracture toughness between two groups (P = 0.05). The mean value of fracture strength for Group A was 721.66 N and for Group B was 396.39 N. Conclusions: Sandblasting improves the bond strength between titanium, and ceramic, mechanical bonding plays a crucial role in the bonding between titanium and ceramic.
Item Description:0972-4052
1998-4057
10.4103/0972-4052.161083