Evaluation of the Bond Strength of Universal Adhesive Systems after Application of 2% Chlorhexidine
Introduction: The influence of chlorhexidine on the bond strength of adhesive systems is still very controversial. Objective: To determine the bond strength of two universal adhesives on dentin after application of 2% chlorhexidine at different application times. Methods: Thirty incisors were used a...
Saved in:
Main Authors: | , |
---|---|
Format: | Book |
Published: |
Editorial Ciencias Médicas,
2024-04-01T00:00:00Z.
|
Subjects: | |
Online Access: | Connect to this object online. |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
MARC
LEADER | 00000 am a22000003u 4500 | ||
---|---|---|---|
001 | doaj_78c9baaf06724c6384aaa1ac9e3b0f8c | ||
042 | |a dc | ||
100 | 1 | 0 | |a María LLashag Bello |e author |
700 | 1 | 0 | |a Marcia Edith Vidalón Pinto |e author |
245 | 0 | 0 | |a Evaluation of the Bond Strength of Universal Adhesive Systems after Application of 2% Chlorhexidine |
260 | |b Editorial Ciencias Médicas, |c 2024-04-01T00:00:00Z. | ||
500 | |a 0034-7507 | ||
500 | |a 1561-297X | ||
520 | |a Introduction: The influence of chlorhexidine on the bond strength of adhesive systems is still very controversial. Objective: To determine the bond strength of two universal adhesives on dentin after application of 2% chlorhexidine at different application times. Methods: Thirty incisors were used and the vestibular surface was abraded to expose the dentin. Subsequently, they were randomly divided into six groups (n = 5). Single Bond Universal (SBU) and All-Bond Universal (ABU) adhesives with/without chlorhexidine were used. Group SBU-0: Single Bond Universal; Group SBU-30: chlorhexidine for 30 seconds + Single Bond Universal; Group SBU-60: chlorhexidine for 60 seconds + Single Bond Universal; Group ABU-0: All-Bond Universal; Group ABU-30: chlorhexidine for 30 seconds + All-Bond Universal and Group ABU-60: chlorhexidine for 60 seconds + All-Bond Universal. Adhesive strength was analyzed by two-factor mixed ANOVA and Tukey's post hoc (p < 0.05). Results: The bond strength for the SBU-60 group increased significantly with respect to the control group (p = 0.032). Similarly, for the ABU-30 and ABU-60 groups, the bond strength increased significantly with respect to the control group (p = 0.001) and (p = 0.000), respectively. Conclusion: Pre-application of 2% chlorhexidine for 60 seconds increases the bond strength of Single Bond Universal and All-Bond Universal adhesive systems. | ||
546 | |a EN | ||
546 | |a ES | ||
690 | |a adhesivo universal | ||
690 | |a clorhexidina | ||
690 | |a fuerza de unión en la dentina. | ||
690 | |a Dentistry | ||
690 | |a RK1-715 | ||
690 | |a Medicine (General) | ||
690 | |a R5-920 | ||
655 | 7 | |a article |2 local | |
786 | 0 | |n Revista Cubana de Estomatología, Vol 61, Iss 0, Pp e4843-e4843 (2024) | |
787 | 0 | |n https://revestomatologia.sld.cu/index.php/est/article/view/4843 | |
787 | 0 | |n https://doaj.org/toc/0034-7507 | |
787 | 0 | |n https://doaj.org/toc/1561-297X | |
856 | 4 | 1 | |u https://doaj.org/article/78c9baaf06724c6384aaa1ac9e3b0f8c |z Connect to this object online. |