Scanning electron microscopic study of teeth restored with fiber posts and composite resin: An in vitro study

Aims and Objectives: The aim of this study is to compare and evaluate the thickness of resin dentin interface zones (RDIZ) obtained by luting carbon fiber post to intra-radicular dentin, either with All-Bond 2 bonding agent and C and B composite cement or Panavia F dentin-bonding system and Panavia...

Full description

Saved in:
Bibliographic Details
Main Authors: K S Sridhara (Author), Sunil Mankar (Author), C M Jayshankar (Author), K Vinaya (Author)
Format: Book
Published: Wolters Kluwer Medknow Publications, 2014-01-01T00:00:00Z.
Subjects:
Online Access:Connect to this object online.
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Aims and Objectives: The aim of this study is to compare and evaluate the thickness of resin dentin interface zones (RDIZ) obtained by luting carbon fiber post to intra-radicular dentin, either with All-Bond 2 bonding agent and C and B composite cement or Panavia F dentin-bonding system and Panavia F resin cement. Materials and Methods: Twenty single rooted mandibular premolars of similar sizes were prepared for the carbon fiber post after biomechanical preparation and obturation. They were divided into two groups, Group 1 and 2 of 10 samples each. Carbon fiber posts used for Group 1 samples were luted using All-Bond 2 and C and B cement. For Group 2 carbon fiber posts were luted using Panavia F dentin-bonding system and Panavia F resin cement. All the 20 samples were sectioned longitudinally and marked at three points on the length of the tooth from the dentin-core interface to the apex at 2 mm, 5 mm, and 8 mm to get coronal, middle, and apical areas, respectively. The formation and thickness (width) of the RDIZ at the marked areas was evaluated by scanning electron microscope using ×1000 magnification. The results were statistical analyzed. Results: Irrespective of the adhesive systems used all specimens showed a RDIZ formation. Microscopic examination of Group 1 showed significantly higher percentage of RDIZ (P < 0.05) than Group 2. RDIZ morphology was easily detectable at coronal and middle areas of all specimens. Conclusion: All-Bond 2 showed denser and wider RDIZ compared with the Panavia F.
Item Description:0975-7406
0976-4879