Hertzian Load-bearing Capacity of Hybrid and Nano-hybrid Resin Composites Stored Dry and Wet
Statement of Problem: Hertzian indentation test has been proven to be an efficient and reliable alternative upon Vickers hardness test. This method has been used to test dental ceramics, amalgams, glass ionomers and luting cements.There is limited published information about the load-bearing capacit...
Saved in:
Main Authors: | Farmani S (Author), Orandi S (Author), Sookhakiyan M (Author), Mese A (Author) |
---|---|
Format: | Book |
Published: |
Shiraz University of Medical Sciences,
2016-03-01T00:00:00Z.
|
Subjects: | |
Online Access: | Connect to this object online. |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Fracture Toughness of Nanohybrid and Hybrid Composites Stored Wet and Dry up to 60 Days
by: Sookhakiyan M, et al.
Published: (2017) -
Relative biocompatibility of micro-hybrid and nano-hybrid light-activated composite resins
by: Abiodun Olabisi Arigbede, et al.
Published: (2017) -
Physical and Mechanical Properties of Bulk-Fill, Conventional, and Flowable Resin Composites Stored Dry and Wet
by: Dana Jafarpour, et al.
Published: (2022) -
Evaluation of the characteristics of nano hybrid composite resin modified with graphene after thermomechanical loading cycle
by: Shameer Muhammad Basheer, et al.
Published: (2023) -
The effect of soda immersion on nano hybrid composite resin discoloration
by: M. Chair Effendi, et al.
Published: (2014)