Effect of Chelating Agents on Push-Out Bond Strength of NeoMTA Plus to Root Canal Dentin
Objective: To evaluate and compare the effect of 17% Ethylenediaminetetraacetic Acid (EDTA), 9% Etidronic acid (HEDP), and 7% Maleic acid (MA) on the push-out bond strength of NeoMTA Plus sealer to the coronal, middle, and apical thirds of root canal dentin. Material and Methods: Forty single-rooted...
Saved in:
Main Authors: | Pattath Kunjan Anju (Author), Tina P. Purayil (Author), Kishore Ginjupalli (Author), Nidambur V. Ballal (Author) |
---|---|
Format: | Book |
Published: |
Association of Support to Oral Health Research (APESB),
2022-01-01T00:00:00Z.
|
Subjects: | |
Online Access: | Connect to this object online. |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Cytotoxicity of NeoMTA Plus, ProRoot MTA and Biodentine on human dental pulp stem cells
by: Sinem Birant, et al.
Published: (2021) -
Biocompatibility of NeoMTA Plus® versus MTA Angelus as delayed furcation perforation repair materials in a dog model
by: Khaled M. Abboud, et al.
Published: (2021) -
Evaluation of push-out bond strength of GuttaFlow 2 to root canal dentin treated with different smear layer removal agents
by: Sree Theja Upadhyay, et al.
Published: (2018) -
Effect of chelating agents on shear bond strength of EpoSeal Plus™ sealer to root canal dentin: In vitro study
by: Prajwal Shetty, et al.
Published: (2021) -
Evaluation of bond strength of splinting materials to the teeth using three adhesive systems-an in vitro study
by: Tina Puthen Purayil, et al.
Published: (2015)