Flexural strengths of reinforced denture base resins subjected to long-term water immersion

Objective This study evaluated the flexural strengths of reinforced denture base resins subjected to long-term water immersion. Materials and methods Acrylic denture base resin reinforced with metal wire or glass fiber-reinforced composite (FRC), and without reinforcement were tested. Bar-shaped spe...

Full description

Saved in:
Bibliographic Details
Main Authors: Kaneyoshi Yoshida (Author), Yutaka Takahashi (Author), Hirono Sasaki (Author), Ippei Hamanaka (Author), Tomohiro Kawaguchi (Author)
Format: Book
Published: Medical Journals Sweden, 2016-12-01T00:00:00Z.
Subjects:
Online Access:Connect to this object online.
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Objective This study evaluated the flexural strengths of reinforced denture base resins subjected to long-term water immersion. Materials and methods Acrylic denture base resin reinforced with metal wire or glass fiber-reinforced composite (FRC), and without reinforcement were tested. Bar-shaped specimens were fabricated. Half of the specimens were stored in 37 °C distilled water for 50 hours (h), the other half were stored in 37 °C distilled water for 180 days (d) before testing. Ten specimens were fabricated per group for each reinforcement/water immersion period combination. The ultimate flexural strength and flexural strength at the proportional limit of reinforced denture base resin were tested. Results The 180 d bulk specimen possessed significantly lower ultimate flexural strength compared with the 50 h bulk specimen (p < 0.05). The ultimate flexural strength of the 50 h metal, 50 h FRC, 180 d metal and the 180 d FRC reinforcement specimens were not significantly different from each other (p > 0.05). The 180 d bulk specimen had a significantly lower flexural strength at the proportional limit compared to the 50 h bulk specimen. The 180 d reinforced specimens of metal and FRC were not significantly different from each of the 50 h specimens. Conclusion The flexural strengths of a reinforced denture base resin did not change after long-term water immersion.
Item Description:2333-7931
10.3109/23337931.2015.1135745