Cellulose isolation from leucaena leucocephala seed: effect on concentration sodium hydroxide / Nur Aini Nabilah Ab Rashid... [et al.]

The isolation of cellulose fibres requires the removal of other components such as lignin, hemicellulose, and pectin from the biomass. In this study, the matured Leucaena leucocephala seeds (LLS) was applied as a raw material to extract cellulose. The influence of sodium hydroxide concentration (2%...

Full description

Saved in:
Bibliographic Details
Main Authors: Ab Rashid, Nur Aini Nabilah (Author), Husin, Maryam (Author), Yury, Norjanah (Author), Othman, Monarita (Author), Mohd Shariff, Zarila (Author), Kassim, Haliza (Author), Li, Abd Rashid (Author)
Format: Book
Published: Universiti Teknologi MARA, Negeri Sembilan, 2019.
Subjects:
Online Access:Link Metadata
Tags: Add Tag
No Tags, Be the first to tag this record!

MARC

LEADER 00000 am a22000003u 4500
001 repouitm_30572
042 |a dc 
100 1 0 |a Ab Rashid, Nur Aini Nabilah  |e author 
700 1 0 |a Husin, Maryam  |e author 
700 1 0 |a Yury, Norjanah  |e author 
700 1 0 |a Othman, Monarita  |e author 
700 1 0 |a Mohd Shariff, Zarila  |e author 
700 1 0 |a Kassim, Haliza  |e author 
700 1 0 |a Li, Abd Rashid  |e author 
245 0 0 |a Cellulose isolation from leucaena leucocephala seed: effect on concentration sodium hydroxide / Nur Aini Nabilah Ab Rashid... [et al.] 
260 |b Universiti Teknologi MARA, Negeri Sembilan,   |c 2019. 
500 |a https://ir.uitm.edu.my/id/eprint/30572/1/30572.pdf 
520 |a The isolation of cellulose fibres requires the removal of other components such as lignin, hemicellulose, and pectin from the biomass. In this study, the matured Leucaena leucocephala seeds (LLS) was applied as a raw material to extract cellulose. The influence of sodium hydroxide concentration (2% - 6%) on the structure of cellulose isolated LLS was studied. The highest yield 23.7% of cellulose was extracted using 4 wt% NaOH treatment. The chemical-physical properties of cellulose extracted were characterized using Fourier Transform Infrared (FTIR), Field Emission Scanning Electron Microscope (FESEM) and X-ray Diffraction (XRD). FTIR spectrum indicated that of all treated samples shows the peaks of cellulose structure. The highest crystallinity index of cellulose was obtained from 6% NaOH treatment which is 76.04%. Under FESEM images, the cellulose appeared in fibrils-like structure. The cellulose obtained can be further disintegrate to micro and nano cellulose to increase the chemical physical properties for various application such as in biocomposite, biomedicine and other value-added chemicals. 
546 |a en 
690 |a QD Chemistry 
690 |a Extraction (Chemistry) 
655 7 |a Article  |2 local 
655 7 |a PeerReviewed  |2 local 
787 0 |n https://ir.uitm.edu.my/id/eprint/30572/ 
787 0 |n https://nsembilan.uitm.edu.my/joacns/ 
856 4 1 |u https://ir.uitm.edu.my/id/eprint/30572/  |z Link Metadata