Effect of Sintering Parameters on Physical Properties of SS 316L Alloy Compact / Mohd Faizul Farhan Ahmad Hamidi..[et al.]

Recently, metal injection moulding (MIM) has been identified as an economical fabrication technique for metal components. MIM, adapted from plastic injection moulding, has four major processing stages, which are: mixing of powder and binder system to produce feedstock, injection moulding, debinding...

Full description

Saved in:
Bibliographic Details
Main Authors: Ahmad Hamidi, Mohd Faizul Farhan (Author), Wan Harun, Wan Sharuzi (Author), Che Ghani, Saiful Anwar (Author), Osada, Toshiya (Author)
Format: Book
Published: Faculty of Mechanical Engineering Universiti Teknologi MARA (UiTM), 2017.
Subjects:
Online Access:Link Metadata
Tags: Add Tag
No Tags, Be the first to tag this record!

MARC

LEADER 00000 am a22000003u 4500
001 repouitm_38684
042 |a dc 
100 1 0 |a Ahmad Hamidi, Mohd Faizul Farhan  |e author 
700 1 0 |a Wan Harun, Wan Sharuzi  |e author 
700 1 0 |a Che Ghani, Saiful Anwar  |e author 
700 1 0 |a Osada, Toshiya  |e author 
245 0 0 |a Effect of Sintering Parameters on Physical Properties of SS 316L Alloy Compact / Mohd Faizul Farhan Ahmad Hamidi..[et al.] 
260 |b Faculty of Mechanical Engineering Universiti Teknologi MARA (UiTM),   |c 2017. 
500 |a https://ir.uitm.edu.my/id/eprint/38684/1/38684.pdf 
520 |a Recently, metal injection moulding (MIM) has been identified as an economical fabrication technique for metal components. MIM, adapted from plastic injection moulding, has four major processing stages, which are: mixing of powder and binder system to produce feedstock, injection moulding, debinding and sintering. In this paper, the physical properties of SS 316L alloy sintered compact sintered at three different sintering parameters were discussed. Thermal properties of the feedstock were characterized by Thermogravimetric Analyzer (TGA) analysis. The debound compacts were sintered at 1100, 1200, and 1300 °C for 3 hours in the high pure argon atmosphere. The heating rate has been set at 10°C/min. The relative density, dimensional shrinkage and microstructure of the sintered compact were investigated. The relative density and dimensional shrinkage increased with the sintering parameters due to high densification of the sintered compact. Some pore sizes seemed to decrease with the increase in sintering temperature. Different sintering temperature shows a significant effect on the physical properties of the sintered compact. 
546 |a en 
690 |a TJ Mechanical engineering and machinery 
655 7 |a Article  |2 local 
655 7 |a PeerReviewed  |2 local 
787 0 |n https://ir.uitm.edu.my/id/eprint/38684/ 
856 4 1 |u https://ir.uitm.edu.my/id/eprint/38684/  |z Link Metadata