Effects of waste paper sludge ash on compressive strength of concrete cubes / Marzuki A.Rahman ...[et al.]

Waste paper sludge incinerator ash (WPSIA) was investigated for its potential use as a replacement for cement in concrete. The physical and chemical properties of raw materials were determined. The water cement ratio was fixed at 0.55 while WPSIA was used at 5%, 10%, 15%, 20%, 25% and 30% replacemen...

Full description

Saved in:
Bibliographic Details
Main Authors: A.Rahman, Marzuki (Author), Hisham, Mohd Syahrul (Author), Jaafar, Mohd Risham (Author), Ruslan, Ahmad (Author), Mohd Saman, Hamidah (Author)
Format: Book
Published: 2006.
Subjects:
Online Access:Link Metadata
Tags: Add Tag
No Tags, Be the first to tag this record!

MARC

LEADER 00000 am a22000003u 4500
001 repouitm_81688
042 |a dc 
100 1 0 |a A.Rahman, Marzuki  |e author 
700 1 0 |a Hisham, Mohd Syahrul  |e author 
700 1 0 |a Jaafar, Mohd Risham  |e author 
700 1 0 |a Ruslan, Ahmad  |e author 
700 1 0 |a Mohd Saman, Hamidah  |e author 
245 0 0 |a Effects of waste paper sludge ash on compressive strength of concrete cubes / Marzuki A.Rahman ...[et al.] 
260 |c 2006. 
500 |a https://ir.uitm.edu.my/id/eprint/81688/1/81688.PDF 
520 |a Waste paper sludge incinerator ash (WPSIA) was investigated for its potential use as a replacement for cement in concrete. The physical and chemical properties of raw materials were determined. The water cement ratio was fixed at 0.55 while WPSIA was used at 5%, 10%, 15%, 20%, 25% and 30% replacement by weight of cement. The grade design of proportions was 30 N/mm2. Slump and compressive strengths were performed on all specimens. Results indicate the WPSA caused a reduction in slump values when it was used as a cement replacement. The replacement of WPSIA up 30% exhibited, generally similar to control mix (0% WPSIA) after 28 days of curing. The maximum compressive strength of 44.1 N/mm2 was achieved using 15% of WPSIA after 60 days of curing. The experimental results presented in this study suggest the potential of WPSIA as a cement replacement. With strength contributing and nontoxic characteristic, the use of WPSIA as a cement replacement may be technically and environmentally feasible. 
546 |a en 
690 |a Industrial and factory wastes 
655 7 |a Conference or Workshop Item  |2 local 
655 7 |a PeerReviewed  |2 local 
787 0 |n https://ir.uitm.edu.my/id/eprint/81688/ 
856 4 1 |u https://ir.uitm.edu.my/id/eprint/81688/  |z Link Metadata