Comparative disintegration rate of non-removable metalceramic prosthesis made of different types of ceramic mass

The frequency of the decay of the ceramic materials used was Vita-95 and Noritake, and methods for their recovery have been proposed. In 119 patients with sintered prosthesis, 63 bridges were examined, 34 of which were made of Noritake and 29 from Vita-95. Of the 56 metal-ceramic crowns, 30 were man...