Carbonization of Asphaltic material and polyethylene by catalysis oxidation V2O5 for activated carbon preparation
The research was aimed to use the residual asphaltic materials taken from northern refinery in the preparation of activated carbon by oxidation with V O5 in the presence of a stream of air for 3hrs at 350°C temp, .The residual materials from primary oxidation and carbonization step was further carbo...