Chapter Formability and Performance of Al-Zn-Mg-Cu Alloys with Different Initial Tempers in Creep Aging Process

The initial temper may directly affect the deformation behavior and material performance in creep age forming (CAF) process. Five heat treatment states are selected as the initial tempers for CAF, namely, solution, peak-aging (T6), over-aging (T73), retrogression and re-solution. The formability and...

ver descrição completa

Na minha lista:
Detalhes bibliográficos
Autor principal: Li, Heng (auth)
Outros Autores: Yang, He (auth), Lei, C. (auth)
Formato: Recurso Electrónico Capítulo de Livro
Idioma:inglês
Publicado em: InTechOpen 2017
Assuntos:
Acesso em linha:OAPEN Library: download the publication
OAPEN Library: description of the publication
Tags: Adicionar Tag
Sem tags, seja o primeiro a adicionar uma tag!

Internet

OAPEN Library: download the publication
OAPEN Library: description of the publication

3rd Floor Main Library

Detalhes do Exemplar 3rd Floor Main Library
Área/Cota: A1234.567
Cód. Barras: 1 Disponível